2011-09-30 Material experiments
Tried a sheet of Dura-Lar clear 0.005. It worked somewhat, but the holograms were much less clear than the styrene, and it felt scratchy while I was working with it. Definitely not the right material for the class.
I also tried a sheet of 0.005 acetate. It was better than the Dura-Lar, but still not quite good enough. The holograms just aren't as bright as those on the styrene(?).